Optical constants of HOYA - BaCD (Dense barium crown)
MC-BACD12
Wavelength:
µm
(0.280 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.468781-0.01062639λ^{2}+0.01325184λ^{-2}+0.0004048612λ^{-4}-2.974799\text{×}10^{-05}λ^{-6}+1.825884\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 3.36e-06 1.02e-08 -4.81e-11 6.1e-07 6.81e-10 4.77e-09 nd: 1.58313 Vd: 59.46 glass_code: 583595 glass_status: standard density: 3.01 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.9e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 9e-06 K-1 dPgF: -0.0008 climatic_resistance: 1.0 stain_resistance: 3.0 acid_resistance: 3.0
Comments
Preforms for Precision molding
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia