Optical constants of HOYA - BaCD (Dense barium crown)
M-BACD15
Wavelength:
µm
(0.280 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.590919-0.01259476λ^{2}+0.01520205λ^{-2}+0.000299998λ^{-4}-1.131547\text{×}10^{-05}λ^{-6}+9.15464\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 7.12968e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.62263 Vd: 58.16 glass_code: 623582 glass_status: standard density: 3.02 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.3e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.2e-06 K-1 dPgF: -0.0045 climatic_resistance: 2.0 stain_resistance: 3.0 acid_resistance: 4.0
Comments
Glass for molded optics lens
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia