Optical constants of HOYA - BaCD (Dense barium crown)
BACD5
Wavelength:
µm
(0.290 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.4861499-0.0095684845λ^{2}+0.014685059λ^{-2}-0.00011216487λ^{-4}+4.1978777\text{×}10^{-05}λ^{-6}-1.885619\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.09e-06 1.25e-08 -4.95e-11 5.43e-07 5.6e-10 1.57e-09 nd: 1.58913 Vd: 61.25 glass_code: 589613 density: 3.27 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.5e-06 K-1 - temperature_range: 20 300 °C coefficient: 6.9e-06 K-1 dPgF: 0.0024 climatic_resistance: 2.0 stain_resistance: 3.0 acid_resistance: 3.0
Comments
General glass Type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia