Optical constants of HOYA - BaCD (Dense barium crown)
BACD4
Wavelength:
µm
(0.300 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.5584621-0.0097457283λ^{2}+0.015110495λ^{-2}+0.00023273333λ^{-4}+1.1137249\text{×}10^{-06}λ^{-6}+1.6424767\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 2.40941e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.61272 Vd: 58.58 glass_code: 613586 glass_status: special density: 3.58 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.6e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.7e-06 K-1 dPgF: 0.0019 climatic_resistance: 2.0 stain_resistance: 4.0 acid_resistance: 4.0
Comments
Not in a position to accept new order because of discontinuation.
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia