Optical constants of HOYA - BaCD (Dense barium crown)
BACD16
Wavelength:
µm
(0.300 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.5859898-0.011940432λ^{2}+0.013995502λ^{-2}+0.00048974502λ^{-4}-3.9120717\text{×}10^{-05}λ^{-6}+2.2611915\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 1.98676e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.62041 Vd: 60.34 glass_code: 620603 density: 3.52 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.1e-06 K-1 dPgF: -0.0003 climatic_resistance: 3.0 acid_resistance: 5.0
Comments
General glass Type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia