Optical constants of HOYA - BaCD (Dense barium crown)
BACD14
Wavelength:
µm
(0.290 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.5335256-0.011903338λ^{2}+0.012257249λ^{-2}+0.00079172149λ^{-4}-7.7381829\text{×}10^{-05}λ^{-6}+3.9935441\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 1.22123e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.60311 Vd: 60.69 glass_code: 603607 density: 3.43 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.4e-06 K-1 dPgF: 0.0019 climatic_resistance: 3.0 stain_resistance: 5.0 acid_resistance: 4.0
Comments
General glass Type
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia