Optical constants of HOYA - BaCD (Dense barium crown)
BACD11
Wavelength:
µm
(0.280 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.4095163-0.0091904415λ^{2}+0.012939968λ^{-2}+0.0002346143λ^{-4}-1.1130589\text{×}10^{-05}λ^{-6}+1.0131863\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 3.66577e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.56384 Vd: 60.83 glass_code: 564608 glass_status: special density: 3.07 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.6e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 7.8e-06 K-1 dPgF: 0.002 climatic_resistance: 1.0 stain_resistance: 2.0 acid_resistance: 2.0
Comments
Not in a position to accept new order because of discontinuation.
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia