Optical constants of HOYA - ADF (Abnormal dispersion flint)
E-ADF50
Wavelength:
µm
(0.350 – 1.550)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.6680422-0.013184258λ^{2}+0.023930479λ^{-2}+0.00023928655λ^{-4}+5.0697941\text{×}10^{-05}λ^{-6}+9.1240958\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 1.08065e-05 0.0 0.0 0.0 0.0 0.0 nd: 1.65412 Vd: 39.62 glass_code: 654396 glass_status: special density: 3.38 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.1e-06 K-1 - temperature_range: 20 300 °C coefficient: 6.5e-06 K-1 dPgF: -0.0033 climatic_resistance: 2.0 acid_resistance: 6.0
Comments
Not in a position to accept new order because of discontinuation.
References
HOYA Zemax catalog 2017-04-01 (obtained from http://www.hoya-opticalworld.com)
Data
INFO
HOYA Corporation
Hoya Corporation is a Japanese company manufacturing optical products.External links
- HOYA Corporation
- HOYA Group Optics DIvision
- HOYA Corporation USA Optics DIvision
- Hoya Corporation - Wikipedia