Optical constants of BARBERINI - Sun Protection
D1616: Grau 1616

Wavelength: µm
 (0.43583 – 0.65627)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Comments

20 ℃
Sun Protection Glass; Colour: greyish-green; Application: dark tinted sunglare filter with high UV- absorption filter category 3 acc. to DIN EN 1836 (for τv > 18 % filter category 2)

References

Barberini D1616 glass specifications, 2010-05

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

Barberini GmbH

Barberini GmbH is a German branch of Barberini S.p.A., the Italian company specializing in ophthalmic materials. Barberini GmbH has been formed after Barberini acquired the ophthalmic division of Schott AG in 2010.