RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

n2 Explorer: Yb:YVO4 (Ytterbium-doped yttrium orthovanadate, Yb:YVO)

Selivanov et al. 2006: n2(o)
Selivanov et al. 2006: n2(e)

LogX   LogY   eV

Details

Selivanov et al. 2006: n2(o)
Selivanov et al. 2006: n2(e)

Reference

Notes

Data




Conditions




Additional information