RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

n2 Explorer: Yb:KY(WO4)2 (Ytterbium doped potassium yttrium tungstate, Yb:KYW)

Selivanov et al. 2006: E∥N_p
Selivanov et al. 2006: E∥N_m
Selivanov et al. 2006: E∥N_g

LogX   LogY   eV

Details

Selivanov et al. 2006: E∥N_p
Selivanov et al. 2006: E∥N_m
Selivanov et al. 2006: E∥N_g

Reference

Notes

Data




Conditions




Additional information