n2 Explorer: Y3Al5O12 (Yttrium aluminium garnet, YAG)

Kabaciński et al. 2019
Adair et al. 1989
Bliss et al. 1974
Owyoung 1973

LogX   LogY   eV

Details

Kabaciński et al. 2019
Adair et al. 1989
Bliss et al. 1974
Owyoung 1973

Reference

Notes

Data




Conditions




Additional information

About Yttrium aluminium garnet

Yttrium aluminium garnet (Y3Al5O12, YAG) is a synthetic crystalline material frequently employed in a variety of applications. It possesses a unique combination of high thermal stability, mechanical robustness, and optical clarity, making it particularly desirable for high-performance environments. In the realm of optics and photonics, YAG is often used as the host crystal in solid-state lasers, most notably the Nd:YAG laser where the YAG crystal is doped with neodymium. These lasers are employed in a range of settings, from medical procedures to material processing. Additionally, undoped YAG is a common substrate for various thin-film applications, given its compatibility with high-temperature deposition processes. In the lighting sector, YAG, when doped with cerium, is used as a phosphor in white LED technology.

Other names and variations

  • Y3Al5O12
  • YAG
  • Yttrium aluminate
  • Yttrium aluminium oxide

Links