RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

n2 Explorer: TlBr-TlI (Thallium bromo-iodide, KRS-5)

Polyanskiy et al. 2024
Jansonas et al. 2022

LogX   LogY   eV

Details

Polyanskiy et al. 2024
Jansonas et al. 2022

Reference

Notes

Data




Conditions




Additional information

About Thallium bromo-iodide

Other names and variations

  • TlBr-TlI
  • KRS-5
  • Thallium bromoiodide
  • Thallium bromide iodide

Links