n2 Explorer: TiO2 (Titanium dioxide)
Adair et al. 1989
LogX
LogY
eV
Details
Reference
Notes
Data
Conditions
Additional information
About Titanium dioxide
Titanium dioxide (TiO2) is a naturally occurring oxide of titanium. It possesses a high refractive index, making it an important material in optical coatings and components, especially as a white pigment in paints, cosmetics, and sunscreens due to its UV absorbing properties. The two main crystal forms used in industry are the rutile and anatase forms. Additionally, its photovoltaic and photocatalytic properties have led to research and applications in solar cells and air purification, respectively. TiO2 also has a robust chemical stability under various conditions, which makes it a preferred material for use in harsh environments.
Minerals: Rutile, Anatase, Brookite.
Other names and variations
- TiO2
- Titanium(IV) oxide
- Titania
- Rutile
- Anatase
- Brookite
Links