n2 Explorer: SiO2 (Silicon dioxide, Silica, Quartz)

Fused silica
VanderLinden et al. 2025
Jansonas et al. 2022
Patwardhan et al. 2021
Kabaciński et al. 2019
Ensley and Bambha 2019
Flom et al. 2015
Milam 1998
DeSalvo et al. 1996
Adair et al. 1989
White et al. 1984
Crystal
Adair et al. 1989: (o)
Adair et al. 1989: (e)

LogX   LogY   eV

Details

Fused silica
VanderLinden et al. 2025
Jansonas et al. 2022
Patwardhan et al. 2021
Kabaciński et al. 2019
Ensley and Bambha 2019
Flom et al. 2015
Milam 1998
DeSalvo et al. 1996
Adair et al. 1989
White et al. 1984
Crystal
Adair et al. 1989: (o)
Adair et al. 1989: (e)