RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

n2 Explorer: Si (Silicon)

Polyanskiy et al. 2024
Jansonas et al. 2022
Ensley and Bambha 2019
Lin et al. 2007
Bristow et al. 2007
Tatsuura et al. 2005; Si[100]
Tatsuura et al. 2005; Si[111]

LogX   LogY   eV

Details

Polyanskiy et al. 2024
Jansonas et al. 2022
Ensley and Bambha 2019
Lin et al. 2007
Bristow et al. 2007
Tatsuura et al. 2005; Si[100]
Tatsuura et al. 2005; Si[111]

Reference

Notes

Data




Conditions




Additional information

About Silicon

Silicon (Si) is a crystalline, brittle element with a bluish-grey metallic luster. It stands as the second most abundant element in the Earth's crust, primarily in the form of silicates and oxides. In its pure form, silicon is employed extensively in the electronics industry for the fabrication of semiconductors, which form the basis of most modern electronic devices. The ability of silicon to act as a substrate for microelectronic devices stems from its semiconductor properties and the potential to precisely dope it with other elements to modify its electrical characteristics. Furthermore, silicon finds use in the photovoltaic industry in solar cells. When it comes to optics, silicon is transparent to infrared light, making it valuable for infrared lenses and other optical components. However, it's opaque to visible light. The material's versatility and abundance have made it integral to many industries, from construction to electronics and beyond

Other names and variations

  • Si
  • Polycrystalline silicon
  • Poly
  • Semicrystalline silicon

Links