RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

n2 Explorer: NaF (Sodium fluoride)

Polyanskiy et al. 2024
Adair et al. 1989
Milam et al. 1977

LogX   LogY   eV

Details

Polyanskiy et al. 2024
Adair et al. 1989
Milam et al. 1977

Reference

Notes

Data




Conditions




Additional information

About Sodium fluoride

Sodium fluoride (NaF) is a white crystalline solid that, when purified, can be processed into transparent optical components. With a broad transparency window spanning from the ultraviolet to the mid-infrared regions, NaF is particularly valuable for certain optical applications, especially in deep ultraviolet systems. However, like some other alkali halides, NaF is sensitive to moisture and can be hygroscopic, making it imperative to ensure proper handling and storage to maintain its optical qualities.

Other names and variations

  • NaF
  • Sodium(I) fluoride

Links