n2 Explorer: NaBr (Sodium bromide)

Adair et al. 1989

LogX   LogY   eV

Details

Adair et al. 1989

Reference

Notes

Data




Conditions




Additional information

About Sodium bromide

Sodium bromide (NaBr) is a white crystalline solid commonly used in various applications. In its pure form, it can be processed into clear crystalline windows or pieces, showcasing transparency not just in the visible range but also extensively into the infrared spectrum. This characteristic transparency in the infrared region is particularly beneficial, making NaBr an invaluable material in infrared spectroscopy and other related optical applications.

Other names and variations

  • NaBr
  • Sedoneural

Links