RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

n2 Explorer: LaF3 (Lanthanum fluoride)

Adair et al. 1989: (o)
Milam et al. 1977: (o)

LogX   LogY   eV

Details

Adair et al. 1989: (o)
Milam et al. 1977: (o)

Reference

Notes

Data




Conditions




Additional information

About Lanthanum fluoride

Lanthanum fluoride (LaF3) is a white, crystalline, inorganic compound that is used in a variety of optical applications. It is a popular choice for the production of fluoride glass and is also used as a scintillation material in radiation detection. Due to its low refractive index, it is often used in antireflection coatings, especially for infrared optics. The compound is stable, has good thermal durability, and exhibits a wide transparency range, making it a versatile material for various optical systems. Its low solubility in water also makes it preferable in moisture-sensitive applications. LaF3 is an important material in both research and commercial optical technologies.

Mineral: Fluocerite-(La)

Other names and variations

  • LaF3
  • Lanthanum trifluoride
  • Lanthanum(III) fluoride
  • Fluocerite-(La)

Links