n2 Explorer: KTaO3 (Potassium tantalate)

Adair et al. 1989

LogX   LogY   eV

Details

Adair et al. 1989

Reference

Notes

Data




Conditions




Additional information

About Potassium tantalate

Potassium tantalate (KTaO3) is a perovskite-structured crystal that has garnered interest in the field of optics and electronics. With its good mechanical and optical properties, KTaO3 serves as a substrate for epitaxial growth of various complex oxides. Additionally, it is used in a variety of applications, including electro-optic modulators, pyroelectric detectors, and nonlinear optics. The material is transparent in the visible and infrared regions, making it valuable for a range of light-based technologies. It is generally non-toxic but should be handled with the usual precautions for chemicals and materials.

Other names and variations

  • KTaO3

Links