RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

n2 Explorer: KCl (Potassium chloride)

Polyanskiy et al. 2021
Adair et al. 1989

LogX   LogY   eV

Details

Polyanskiy et al. 2021
Adair et al. 1989

Reference

Notes

Data




Conditions




Additional information

About Potassium chloride

Potassium chloride (KCl) is a salt that finds use in various optical applications due to its wide spectral transmission range. Like its bromide counterpart, potassium chloride is hygroscopic, requiring cautious handling and storage conditions to preserve its optical qualities. It is commonly used as a prismatic or plane-parallel component in infrared spectroscopy, particularly because of its low cost and good transmission in the mid and far-infrared regions. Additionally, it serves as a substrate for specialized optical coatings. Due to its moisture sensitivity, it's less suitable for applications exposed to high humidity or varying environmental conditions. Nonetheless, KCl remains an important material in the toolkit of optical engineers and scientists.

Other names and variations

  • KCl

Links