Adair et al. 1989

LogX   LogY   eV

Details

Adair et al. 1989

Reference

Notes

Data




Conditions




Additional information

About Gadolinium scandium aluminium garnet

Gadolinium scandium aluminium garnet (Gd3Sc2Al3O12, or GSAG) is a synthetic garnet crystal known for its excellent thermal properties and broad transparency range in the visible and near-infrared regions. This material has a refractive index of around 1.97 in the 632.8 nm wavelength and is characterized by its thermal and mechanical robustness. GSAG serves as a substrate for the epitaxial growth of other garnet crystals and is also utilized in high-temperature applications. The material's stability and favorable optical properties make it a candidate for use in various optical components, such as laser hosts and optical isolators, particularly in systems that operate under demanding conditions.

Other names and variations

  • Gd3Sc2Al3O12
  • GSAG