n2 Explorer: CeF3 (Cerium trifluoride)

Adair et al. 1989: (o)
Milam et al. 1977

LogX   LogY   eV

Details

Adair et al. 1989: (o)
Milam et al. 1977

Reference

Notes

Data




Conditions




Additional information

About Cerium trifluoride

Cerium fluoride (CeF3) is an inorganic compound that crystallizes in the hexagonal or orthorhombic structure. This material is notable for its scintillating properties, which makes it particularly useful in radiation detection applications such as medical imaging and high-energy physics experiments. With a high atomic number and a high density, CeF3 is very effective at stopping high-energy photons, thereby converting their energy into a detectable light signal. It has a fast decay time, which is crucial for time-resolved measurements. Additionally, cerium fluoride is chemically stable and non-hygroscopic, an important feature for long-term operational reliability. While it is generally less expensive than other rare-earth scintillators, the challenge lies in optimizing its light yield and improving the energy resolution of detectors in which it is used. Synthesis methods for CeF3 include solid-state reaction, hydrothermal processes, and co-precipitation, with each offering different advantages in terms of crystal quality and purity. Overall, CeF3 remains a material of interest for various optoelectronic applications and continues to be the subject of research aimed at optimizing its scintillating properties.

Mineral: Fluocerite-(Ce)

Other names and variations

  • CeF3
  • Cerium(III) fluoride
  • Cerium fluoride
  • Fluocerite-(Ce)