RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

n2 Explorer: CdTe (Cadmium telluride)

Tatsuura et al. 2005; CdTe[100]
Tatsuura et al. 2005; CdTe[111]
Sheik-Bahae et al. 1991

LogX   LogY   eV

Details

Tatsuura et al. 2005; CdTe[100]
Tatsuura et al. 2005; CdTe[111]
Sheik-Bahae et al. 1991

Reference

Notes

Data




Conditions




Additional information

About Cadmium telluride

Cadmium telluride (CdTe) is an inorganic compound that typically crystallizes in a cubic zincblende structure. It is a direct bandgap semiconductor with a bandgap energy of approximately 1.5 eV, making it highly suitable for photovoltaic applications, especially thin-film solar cells. CdTe solar cells are commercially significant due to their lower manufacturing costs and competitive efficiency levels compared to silicon-based cells. Besides photovoltaics, CdTe is also employed in infrared detectors, radiation detectors, and electro-optic modulators. However, the presence of cadmium, a toxic heavy metal, calls for stringent handling and disposal protocols and has prompted research into recycling methods. Synthesis methods for CdTe include physical vapor deposition, chemical vapor deposition, and close-spaced sublimation, among others, each offering unique advantages in terms of film quality and manufacturing scalability. Despite the environmental concerns related to its toxicity, CdTe remains a highly relevant material in renewable energy technologies and continues to attract research efforts aimed at mitigating its environmental impact.

Other names and variations

  • CdTe

Links