RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

n2 Explorer: BaGa4Se7 (Barium gallium selenide, BGSe)

Jansonas et al. 2022

LogX   LogY   eV

Details

Jansonas et al. 2022

Reference

Comments

Data




Conditions




Additional information

About BaGa4Se7

BaGa4Se7, commonly abbreviated as BGSe, is a chalcogenide-based nonlinear optical crystal known for its phase-matching capabilities and broad transparency window. This material is particularly suited for frequency conversion applications in the mid-infrared region, including second-harmonic generation (SHG), sum-frequency generation (SFG), and optical parametric oscillation (OPO). BGSe exhibits high nonlinear optical coefficients, as well as a high laser damage threshold, making it well-suited for high-power applications. The crystal is generally grown using techniques like the Bridgman-Stockbarger method, and can be cut and polished into high-quality facets for optimal performance. One important consideration for this material is its sensitivity to moisture and other environmental factors; thus, careful handling and storage are required to maintain its optical properties. Overall, BGSe offers a compelling combination of properties that make it a valuable material for nonlinear optics, especially for applications requiring high efficiency and broad tunability in the mid-infrared range.

Other names and variations

  • BGSe

Links