n2 Explorer: BaF2 (Barium fluoride)
Polyanskiy et al. 2021
Ensley and Bambha 2019
DeSalvo et al. 1996
Sheik-Bahae et al. 1991
Adair et al. 1989
Milam et al. 1977
Details
Reference
Comments
Data
Conditions
Additional information
About Barium fluoride
BaF2, or barium fluoride, is a crystal that offers a wide transmission range, spanning from the ultraviolet into the mid-infrared regions. This material is commonly used in specialized optical applications such as scintillators in high-energy physics experiments, and as windows and lenses in infrared spectroscopy systems. It possesses a relatively low refractive index and high resistance to radiation damage, which makes it especially useful in extreme conditions. Additionally, BaF2 has fast scintillation response times, making it advantageous in fast-timing applications. One drawback, however, is that the crystal is hygroscopic, making it sensitive to moisture and requiring proper storage and handling to maintain its optical properties. It also has a lower resistance to thermal and mechanical shock compared to other fluoride crystals, which can be a consideration depending on the intended application. Despite these limitations, BaF2 remains a highly valuable material for specialized optical and photonic applications, owing to its broad transmission range and resilience to high-energy radiation.
Other names and variations
- BaF2
- Barium difluoride
- Barium(II) fluoride
Links