n2 Explorer: AlN-Al2O3 (Aluminium oxynitride, ALON)

Flom et al. 2015

LogX   LogY   eV

Details

Flom et al. 2015

Reference

Notes

Data




Conditions




Additional information

About Aluminium oxynitride

Other names and variations

  • AlON
  • ALON

Links