Optical constants of Micro resist ma-N 405 : ma-T 1050, 1:1
Sarkar et al. 2019: n,k 0.375–1.69 µm

Wavelength: µm
 (0.3750–1.6900)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Comments

Spin-coated negative photoresist ma-N 405 diluted with ma-T 1050 (micro resist technology GmbH) in a 1:1 ratio.

References

S. Sarkar, V. Gupta, M. Kumar, J. Schubert, P.T. Probst, J. Joseph, T.A.F. König. Hybridized guided-mode resonances via colloidal plasmonic self-assembled grating. ACS Appl. Mater. Interfaces, 11, 13752-13760 (2019) (Numerical data kindly provided by Dr. Tobias König)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Resists

In semiconductor fabrication, a resist is a thin layer used to transfer a circuit pattern to the semiconductor substrate which it is deposited upon. (from Wikipedia)

Links: