Sarkar et al. 2019: n,k 0.301–1.69 µm

Wavelength: µm
 (0.3014–1.6880)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

film_thickness: 1.0E-6
substrate: glass

Comments

Negative tone resist (ma-N 1407) thin film (thickness 1000 nm) on glass substrate.

References

S. Joseph, S. Sarkar, J. Joseph. Grating-coupled surface plasmon-polariton sensing at a flat metal–analyte interface in a hybrid-configuration. ACS Appl. Mater. Interfaces, 12, 46519-46529 (2020) (Numerical data kindly provided by Prof. Joby Joseph)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Resists

In semiconductor fabrication, a resist is a thin layer used to transfer a circuit pattern to the semiconductor substrate which it is deposited upon. (from Wikipedia)

Links: