Optical constants of Micro resist EpoCore
Spec sheet: n 0.45–1.55 µm

Wavelength: µm
 (0.45–1.55)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.572+0.0076λ^{-2}+0.00046λ^{-4}$$

Comments

Micro resist EpoCore negative photoresist for waveguide manufacturing

References

Micro resist EpoCore and EpoClad datasheet, 2015