Optical constants of Biodisel
Wang et al. 2015: 20 °C; n,k 0.300–2.50 µm
Wavelength:
µm
(0.300–2.500)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions
temperature: 293
Comments
Biodiesel, 20 °C.
References
C. C. Wang, X. C. Li, J. Y. Tan, L. H. Liu. Experimental measurement of optical constant of biodiesel by double optical pathlength transmission method. Laser Optoelectron. Prog. 52, 051206 (2015) (Numerical data kindly provided by Chengchao Wang)
Data
Additional information
About Biodisel
Links: