Optical constants of Zr-H (Zirconium-hydrogen alloy, Zirconium hydride)
Palm et al. 2018: n,k 0.226-1.68 µm
Wavelength:
µm
(0.226076263 – 1.684528687)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
Zirconium Hydride, Under 7 bar H2 gas, Room temperature, 200 nm thin film, electron beam evaporated, vacuum annealed 2 hr 350 °C.
References
K. J. Palm, J. B. Murray, T. C. Narayan, J. N. Munday. Dynamic optical properties of metal hydrides, ACS Photonics 5, 4677-4686 (2018)
(Numerical data kindly provided by Kevin Palm)