Optical constants of ZnO-CdO (Zinc cadmium oxide, ZnCdO)
Aguilar et al. 2019: n,k 0.3–3.2 µm; 10% ZnO
Wavelength:
µm
(0.300 – 3.200)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
Zn0.1Cd0.9O (10% ZnO, 90% CdO) thin film.
References
O. Aguilar, S. de Castro, M. P. F. Godoy, M. R. S. Dias. Optoelectronic characterization of Zn1-xCdxO thin films as an alternative to photonic crystals in organic solar cells, Opt. Mater. Express 9, 3638-3648 (2019) (Numerical data kindly provided by Mariama Rebello de Sousa Dias)
Data
INFO
Zinc-cadmium oxide - ZnCdO (ZnO-CdO)
Other names
ZnO other names:- Zinc white
- Calamine
- Philosopher's wool
- Chinese white
- Flowers of zinc
- Cadmium(II) oxide
- Cadmium monoxide