Optical constants of V-Ga (Vanadium-gallium alloy)
Golovashkin et al. 1970: n,k 0.45-2.6 µm; 78 K
Wavelength:
µm
(0.45 – 2.60)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
temperature: 78 K
Comments
78 K (-195.15 °C). Avaraged data for samples containing 37, 33, and 6 wt% gallium (optical constants of the three samples are close to one another).
References
A. I. Golovashkin, I. S. Levchenko and G. P. Motulevich. Optical properties and electron characteristics of vanadium-gallium alloys obtained by evaporation in vacuum, Sov. Phys. JETP 30, 44-48 (1970)
Data
INFO
Vanadium-gallium alloy, V-Ga
Other names
- Vanadium gallide
- Trivanadium monogallide (only for V3Ga compound)