Optical constants of TL-216
Li et al. 2005: n(e) 0.450–0.656 µm

Wavelength: µm
 (0.45–0.656)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.6772+0.0155λ^{-2}+0.0011λ^{-4}$$

Conditions

temperature: 298
optical_component: e

Notes

25 °C. Extraordinary optical constants (e).

References

J. Li, C. H. Wen, S. Gauza, R. Lu, S. T. Wu. Refractive indices of liquid crystals for display applications. J. Disp. Technol. 1, 51-61, 2005