Optical constants of Surlyn A-1601
Smith and Loewenstein 1975: n,k 28.6–200 µm
Wavelength:
µm
(28.5714–200.0000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
Ionomer resin manufactured by DuPont under the name Surlyn A-1601.
References
D. R. Smith and E. V. Loewenstein. Optical constants of far infrared materials. 3: plastics. Appl. Opt. 14, 1335-1341 (1975)
Data
Additional information
About Surlyn
Surlyn is the brand name of an ionomer resin created by DuPont, a copolymer of ethylene and methacrylic acid used as a coating and packaging material.