Optical constants of Si-O (Non-stoichiometric silicon oxide)
Herguedas and Carretero 2023: SiO1.92; n,k 5.0–25 µm
Wavelength:
µm
(5.000–25.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_is_absolute: true wavelength_is_vacuum: true
Comments
SiO1.92. Sputtered Si with 120 sccm O2 and 80 sccm Ar, which is equivalent to a oxygen partial pressure of 7.3 × 10-4 mbar and a total pressure of 1.5 × 10-3 mbar. Room temperature.
References
N. Herguedas and E. Carretero. Optical properties in mid-infrared range of silicon oxide thin films with different stoichiometries, Nanomaterials 13, 2749 (2023)