Optical constants of Si-Ge (Silicon-germanium, SiGe)
Jellison et al. 1993: 47% Si, Si substrate; n,k 0.24-0.84 µm
Wavelength:
µm
(0.240 – 0.840)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: false x: 0.47 thickness: 7 μm substrate: Si
Comments
SixGe1-x, x = 0.47. 7-μm film grown on Si substrate.
References
G. E. Jellison Jr., T. E. Haynes, H. H. Burke. Optical functions of silicon-germanium alloys determined using spectroscopic ellipsometry, Opt. Mat. 2, 105-117 (1993)