Optical constants of P3HT:PC61BM
Stelling et al. 2017: n,k 0.247-1.685 µm
Wavelength:
µm
(0.24718 – 1.68492)
Derived optical constants
n
k
logX
logY
eV
Comments
Isotropic P3HT:PC61BM thin film (thickness 80 nm) on silicon substrate.
References
C. Stelling, C. R. Singh, M. Karg, T. A. F. König, M. Thelakkat, M. Retsch. Plasmonic nanomeshes: their ambivalent role as transparent electrodes in organic solar cells, Sci. Rep. 7, 42530 (2017) - see Supplementary information (Numerical data kindly provided by Tobias König)
Data
INFO
P3HT:PC61BM
Applications
- Solar cells
Chemical composition
P3HT: (C41H53FO4S4)n PC61BM: C72H14O2Other names (P3HT)
- Poly(3-hexylthiophene-2,5-diyl)
- Plexcore OS 2100
Other names (PC61BM)
- [6,6]-phenyl-C61-butyric acid methyl ester