Optical constants of Norland NOA 61
Norland spec sheet: Cured; n 0.450–1.55 µm

Wavelength: µm
 (0.45–1.55)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.5375+0.00829045λ^{-2}-0.000211046λ^{-4}$$

References

Norland Optical Adhesive 61 Data 1, Data 2 (accessed 2016-04-20)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]