Optical constants of Microchem SU-8 2000
Spec sheet: n 0.32–0.80 µm

Wavelength: µm
 (0.32–0.8)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.566+0.00796λ^{-2}+0.00014λ^{-4}$$

Comments

Microchem SU-8 2000 permanent epoxy negative photoresist. Uncured.

References

Microchem SU-8 2000 Data Sheet, 2011