Optical constants of Microchem 8.5 mEL copolymer resist
Spec sheet: n 0.2–1.1 µm

Wavelength: µm
 (0.2–1.1)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.478+0.0007204λ^{-2}+0.0003478λ^{-4}$$

Comments

Microchem 8.5 mEL copolymer resist

References

Microchem PMMA Datasheet, 2001

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]