RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of Leica Type F
Wang et al. 2017: k 1.2–1.9 µm

Wavelength: µm
 (1.200–1.900)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

temperature: 295

Comments

22 °C.

References

K. Wang, W. Wen, Y. Wang, K. Wang, J. He, J. Wang, P. Zhai, Y. Yang, P. Qiu. Order-of-magnitude multiphoton signal enhancement based on characterization of absorption spectra of immersion oils at the 1700-nm window. Opt. Express 25, 5909-5916 (2017)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]