Optical constants of Kapton
Arakawa et al. 1981: n 0.02–1.49 µm, k 0.02–0.43 µm

Wavelength: µm
 (0.02–1.49)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Comments

Kapton type H polyimide film

References

E. T. Arakawa, M. W. Williams, J. C. Ashley, L. R. Painter. The optical properties of Kapton: Measurement and applications. J. Appl. Phys. 52, 3579-3582 (1981)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Kapton

Kapton is a polyimide film developed by DuPont in the late 1960s that remains stable across a wide range of temperatures.