Optical constants of Hydrogenated amorphous carbon
Smith 1984: As-deposited; n,k 0.261–0.827 µm
Wavelength:
µm
(0.261 – 0.827)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
wavelength_vacuum: true substrate: fused_quartz
Comments
As-deposited (Td = 250 ℃)
References
F. W. Smith. Optical constants of a hydrogenated amorphous carbon film, J. Appl. Phys. 55, 764 (1984)