Optical constants of H2O:C3H5(OH)3 (Water:Glycerol)
Gupta et al. 2022: n 0.40–0.71 µm; 100 wt% glycerol
Wavelength:
µm
(0.4 – 0.71)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n=1.46004+3.94934611\text{×}10^{-3}λ^{-2}-1.77343\text{×}10^{-5}λ^{-4}$$Comments
Room temperature.
References
V. Gupta, O. Aftenieva, P. T. Probst, S. Sarkar, A. M. Steiner, N. Vogel, A. Fery, T. A. F. König. Advanced colloidal sensors enabled by an out-of-plane lattice resonance, Adv. Photonics Res. 2022, 2200152 (see supporting information)