Optical constants of GaP-InP (Gallium indium phosphide, GaInP)
Schubert et al. 1995: n,k 0.250–0.954 µm

Wavelength: µm
 (0.24961–0.95395)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Comments

Ga0.51In0.49P; Eg=1.85±0.2 eV; Room temperature.

References

M. Schubert, V. Gottschalch, C. M. Herzinger, H. Yao, P. G. Snyder, J. A. Woollam. Optical constants of GaxIn1−xP lattice matched to GaAs. J. Appl. Phys. 77, 3416 (1995)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]