Optical constants of GaAs-InAs (Gallium indium arsenide, GaInAs)
Adachi 1989: n,k 0.207-12.4 µm
Wavelength:
µm
(2.0664e-01 – 1.2398e+01)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
In1-xGaxAs; x=0.48
References
S. Adachi. Optical dispersion relations for GaP, GaAs, GaSb, InP, InAs, InSb, AlxGa1−xAs, and In1−xGaxAsyP1−y, J. Appl. Phys. 66, 6030-6040 (1989)
[Calculation script (Python)]
Data
INFO
Gallium indium arsenide, GaInAs
Other name
- Indium gallium arsenide, InGaAs