RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optica Laser Congress

Optical constants of E7
Tkachenko et al. 2006: n(e) 0.532–1.7 µm

Wavelength: µm
 (0.532–1.7)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.67798+0.01696λ^{-2}+0.00127λ^{-4}$$

Conditions

direction: e

Comments

Extraordinary ray (e).

References

V. Tkachenko, G. Abbate, A. Marino, F. Vita, M. Giocondo, A. Mazzulla, F. Ciuchi, L. De Stefano. Nematic liquid crystal optical dispersion in the visible-near infrared range. Mol. Cryst. Liq. Cryst. 454, 263/[665]-271/[673], 2006