Optical constants of Cu-Zn (Copper-zinc alloy, Brass)
Querry 1985: n,k 0.21-55.6 µm; 90% Cu 10% Zn
Wavelength:
µm
(0.2100 – 55.5556)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
90% Cu, 10% Zn.
References
M. R. Querry. Optical constants, Contractor Report CRDC-CR-85034 (1985)